>Yes. This can be done. Sorted fasteners, not too pitted can be taken to
>platers where they can be yelllow zinkdicromated to look like new. Most
>platers will charge a batch charge...or charge you a flat fee for lets say
>a 5 gallon bucket full.

Yes indeed, the only thing I can add is that if you bead blast (glass) the
parts then have them plated they look really nice. Lot charges around here
for yellow dichromate zinc are around $50.

je